Kinetic Metallization vs. Hard Chrome Replacement
|
Post-Test Roughness Ra, µin |
|
17 |
61 |
|
Hard Cr |
>200 |
21 |
OEM |
>200 |
22 |
For more information on our Tungsten Carbide Cobalt powder click here.